How to specify shrinkage so garments still fit after washing
· 3 min read
Wash the sample before you measure it, put washed measurements in the tech pack and write a residual shrinkage limit of 3%, tested and in writing, because cotton can shrink 3 to 5% on a body length.
On this page
Why did my garment shrink when the sample measured correctly?
Because the sample, the bulk and your approval were all measured dry, and your customer measures after a wash. The factory met the specification; the specification said nothing about washing.
Here is how it happens. The sample body length measures 71 cm, exactly the spec, and you approve it. Bulk arrives at 71 cm. Nobody in the chain has done anything wrong. Then the customer washes the garment once, and it comes back at 68 cm.
Three centimetres is the gap between the garment you approved and the garment your customer actually owns. It is a common fit complaint, and it is common precisely because every check before delivery was a check on a garment that had not yet been washed.
How much does cotton shrink?
Cotton shrinks, and 3 to 5% on a body length is a realistic range. On a garment of this length that is two to three centimetres, which is most of a size.
Shrinkage is not one fixed number for a fabric. It moves with:
- the fibre,
- the construction, knit or woven,
- the finish the fabric has been given,
- and how the garment is dried.
The last of those belongs to the customer, not to you. The same cotton jersey can behave quite differently depending on whether it goes in a tumble dryer or is laid flat:
| Drying | Shrinkage on a cotton jersey (working example) |
|---|---|
| Tumble dried | might be 4% |
| Dried flat | might be 1.5% |
These figures illustrate how wide the range can be; they are not results for any particular fabric. The point is that a garment does not have one shrinkage. It has a range, and part of that range is decided in somebody else's laundry. A specification has to allow for that rather than assume the gentlest case.
Is shrinkage a factory defect?
Not if you never specified it. Your specification is the only thing a factory has to meet, and if the wash is not in it, the shrinkage is yours.
That can feel unfair, because the customer does not care whose responsibility it was. But from the factory's side the order was delivered to the measurements agreed. A complaint about a garment that met its spec is a complaint about the spec, and the fix is not a better argument after delivery. It is a line in the tech pack before the order.
Does “pre-shrunk” mean the garment will not shrink?
On its own, it means very little. It says the fabric or garment went through some shrinkage treatment; it does not say how much movement is left.
What you need instead is a residual shrinkage maximum: the amount the garment may still move after the factory's own finishing. A working limit is 3%, tested and in writing. Without a number like that you have not specified shrinkage. You have only mentioned it.
A residual limit turns a vague promise into something that can be measured, passed or failed, and that both sides agreed before production started.
How do I wash-test a sample?
Ask for a wash test, not a promise: three pieces, three wash cycles, measured before and after, with the numbers written down. It costs a sample and an afternoon.
To make the result useful:
- Measure the same points every time: the body length, the chest and any measurement the fit depends on.
- Record how the pieces were dried, since drying changes the result.
- Compare the washed measurements with your specification, not with the dry sample.
Then wash the sample you are approving, measure it, and approve the washed garment. If it comes out of the wash at the right size, you know what your customer will own. If it does not, you have found out at the stage where the pattern can still change.
Should the tech pack hold washed or dry measurements?
Washed. Put washed measurements in the tech pack, not dry ones, so the specification describes the garment the customer will wear rather than the one that leaves the factory.
That changes what the factory is aiming at. A spec written dry is met by a garment that is right until its first wash. A spec written washed has to be met after the wash, which means the shrinkage has to be accounted for in the pattern and the fabric choice, where it can be.
How should bulk be checked for shrinkage?
Measure the bulk washed. If your quality control measures dry and your customer measures after a wash, you are checking a garment nobody owns.
A few pieces from the delivery, washed and then measured against the washed measurements and the residual limit, tell you whether production behaves the way the sample did. A dry measurement alone tells you the garment was sewn to size, which is useful, but it answers only half the question.
What to write in the tech pack
- Washed measurements, not dry ones.
- A residual shrinkage limit, for example 3%, with the test it is measured by.
- The wash test: number of pieces, number of cycles, how they are dried and which points are measured.
- A washed bulk check, so delivery is measured the way your customer will measure it.
Before signing off a sample, read how to budget and approve a sample. If the specification is still to be written, start with a free tech pack.